Features | Application Procedure
| Product / Product Description |
Hardner Mixing Ratio |
Packing |
Thinner Recommended |
Thinner Intake |
Area of Application |
Drying Time |
| Spray |
Brush |
Roller |
Touch |
Hard |
| TreatWood Sealer Clear |
3:1 |
Two |
Thinner 3830 |
30-35% |
- |
- |
Interior wood |
25min |
8hrs |
| Thinner 3831 |
- |
20-25% |
| Treat Wood Glossy Clear |
3:1 |
Two |
Thinner 3830 |
25-30% |
- |
- |
Interior wood |
30min |
8hrs |
| Thinner 3831 |
- |
15-20% |
- |
- |
- |
- |
| Treat Wood Matt Clear |
5:1 |
Two |
Thinner 3830 |
25-30% |
- |
- |
Interior wood |
30min |
8hrs |
| Thinner 3831 |
- |
15-20% |
- |
- |
- |
- |
Clean the existing surface thoroughly with emery paper 36/80/120 to make the surface smooth.
- Apply two coats of Treat Wood Sealer either by spray or brush between two coats. Allow it to dry for 8hrs or overnight.
- Sand the first coat by 220 emery paper.
- Apply the second coat and sand the surface by 320 emery papers.
- Apply two coats of TreatWood Sealers and MRF Wood Stains.
- Note: for colouring/Staining the wood, use MRF Wood Stains.
- Apply the stainer either by applying by cloth or mixing in top coat clear (Matt or Glossy).
- Don't sand the stained wood.
- Apply two coats of Treat wood Glossy or Matt Clear or intermixing the two, to have the desired gloss level.
- Between two coats, allow drying time of 8hrs, or overnight.
- Sand the first coat of top coat clear by 400 emery paper.
[Disclaimer: The manufacturer reserves the right to change the specification without prior notice]
|